We did this exercise in 2004 when we converted our old 125t/h, single string cyclone preheater kiln into a 36t/h lime kiln. However, the Metso limestone preheater was sized for a specific lime market volume, not the actual maximum possible capacity of the kiln, which is estimated at about 80t/h.
The old cyclone ...
-
MgO enters into solid solution in all the cement clinker minerals to different degrees. In these solid solutions it essentially substitutes for CaO. The convention is that up to 2% MgO can be accommodated in solid solution in the clinker minerals. Beyond 2% there is the likelihood that free MgO will be present and then there is the possibility of ...
|
|
|