free lime

dear all how to contol free lime in clinker

Reply


Know the answer to this question? Join the community and register for a free guest account to post a reply.

usman2978
6 posts
TimePosted 12/03/2012 17:23:33
usman2978 says

re free lime

there are following possibilities.

1-varition in kiln feed LSF

2-co formation

3-clinker cooling

4-Fe2O3 high content in kiln feed

5-high liquid phase

6-flame shape not coorect.