Re: Clinker nodulization

Dear Dr. Zoey I want to type a part from the Taylor "Cement Chemistry": "Nodulization requires an adequate proporti...

Re: Reduction in clinker production

In the case you explained, the core of clinker must be brown. Chek in your clinker FeO content (it must be high als...

Re: clinker storage

Dear Azhar, I can add only to our friends' opinions that outside storing of clinker lead to partial hydration of cli...

Re: clinker factor

Dear elwathig, there is no any limitation or allowness regarding conversion factor. Less the conversion factor is be...

Re: kiln hood draft

Dear elwathig I'll try to answer. If you want to know real connection, you should go to your cotrol room and close ...

Re: Clinker Grindability

Dear Shyam for detailed answer I need to know from you LSF and free lime content in clinker also. And it will be bet...

Re: Issues with a product made with White Cement

I agree with Ted. The problem you described, maybe because of content of CaCl2, maybe you have to decrese the conten...

Re: high free lime

Dear Bazarah Our colleagues mentioned many cases that could cause unnormal burning. I want to add something: you ca...

Re: Alkalies in pozzolans

Hi Ted Thank you for your answer. You've confirmed my point of view, so I've already sent samples of the pozzolans ...

Re: spec for cement type is OPC 42.5-R. 3200 softness

Dear svr 1954  In 42.5R  42.5 is 42.5 MPa or 433 kg/sm2 that means that the cement compressive stength after 28 d...