the role of CaF2 addition in white cement clinker production

Dear all, Kindly I would like to know the role of CaF2 addition in clinker production of white cement and also its ...

alk-sulphate single salts

Dear All , kindly i want to clarify info. about Alk-sulphate ( Na2SO4 & K2SO4 ) these compounds share in build up ...

Re: Coating formation in Kiln Inlet

Dear All ,   kindly i want to clarify info. about Alk-sulphate ( Na2SO4 & K2SO4 )  these compounds share in buil...

Re: Clinker High Liter Weight and High Free Lime

Dear Mr. Raj Kindly , to privent miss understanding , you want to say that higher finess material  ( lower sieve r...

Re: Clinker High Liter Weight and High Free Lime

Dear Mr. Raj  i am diss agree with u cos we have sieve residue of 90 micron = 24.0 % and 212 micron = 8 % and we do...

Re: Clinker High Liter Weight and High Free Lime

Dear Mr. Raj. i would like to know why the material hard to burn despite the sieve residue  212 = 1.6 % and even 90...

separation factor

Dear All ,  i would like to know what is the separation factor of the silo ( cf silo ) of rawmaterial ( KF) and how...

Re: coating problem

our thik coat found in the burning zone and ther is a middle ring in the end of  transition zone  

coating problem

Dear All  we have a problem in our kiln coat , the problem represent in that the coat thikness exceed 50 cm ( abou...

burning zone coat formation

Dear All ,  kindly i would like to know the mechanism of coat formation specialy in the burning zone ( from chemica...